Hydro-Thermal Fatigue of Polymer Matrix Composite Biomaterials.

Opis bibliograficzny

Hydro-Thermal Fatigue of Polymer Matrix Composite Biomaterials. [AUT.] PIENIAK DANIEL, PRZYSTUPA KRZYSZTOF, WALCZAK AGATA, NIEWCZAS AGATA M., KRZYŻAK ANETA, BARTNIK GRZEGORZ, GIL LESZEK, LONKWIC PAWEŁ. Materials. DOI: 10.3390/ma12223650
Skopiowane!
Kliknij opis aby skopiować do schowka

Szczegóły publikacji

Źródło:
Rok:2019
Język:angielski
Charakter formalny:Artykuł w czasopismie
Typ MNiSW/MEiN:inne

Streszczenia

This study discusses a quantitative fatigue evaluation of polymer–ceramic composites for dental restorations, i.e., commercial (Filtek Z550) and experimental Ex-nano (G), Ex-flow (G). Their evaluation is based on the following descriptors: mechanical strength, elastic modulus and strain work to fracture. Supposed to reflect factors of environmental degradation conditions, thermal fatigue was simulated with a special computer-controlled device performing algorithms of thermocycling. The specimens intended for the strength test underwent 104 hydro-thermal fatigue cycles. This procedure of thermocycling was preceded by aging, which meant immersing the specimens in artificial saliva at 37 °C for 30 days. The strength tests after aging only and after aging and thermocycles were performed in line with the three-point flexural strength (TFS) test, specified in ISO 4049, and the biaxial flexural strength (BFS) test, specifically piston-on-three-ball in accordance with ISO 6872. Based on the results, it can be stated that composites with higher volume content of inorganic particles after aging only show higher strength than materials with lower filler particle content. For example, the average flexural bending strength of the Ex-flow (G) composite was about 45% lower than the value obtained for the Ex-nano (G) material. The residual strength after thermocycles is significantly lower for the experimental composites, whereas a smaller decrease in strength is recorded for the commercial composites. Decreases in strength were about 4% (Filtek Z550), 43% (Ex-nano (G)), and 29% (Ex-flow (G)) for the BFS test; and about 17% (Filtek Z550), 55% (Ex-nano (G)), 60% (Ex-flow (G)) for the TFS test. The elastic modulus of the experimental composites after only aging is higher (about 42%) than that of the commercial composite, but the elastic modulus of the commercial composite increases significantly after thermocycling. A descriptor known as strain work to fracture turns out to be a good descriptor for evaluating the hydro-thermal fatigue of the tested polymer–ceramic composites

Identyfikatory

ISSN: 1996-1944
BPP ID: (7, 8236) wydawnictwo ciągłe #8236

Metryki

140,00
Punkty MNiSW/MEiN
0
Impact Factor
0
Index Copernicus
0
Punktacja wewnętrzna

Eksport cytowania

Wsparcie dla menedżerów bibliografii:
Ta strona wspiera automatyczny import do Zotero, Mendeley i EndNote. Użytkownicy z zainstalowanym rozszerzeniem przeglądarki mogą zapisać tę publikację jednym kliknięciem - ikona pojawi się automatycznie w pasku narzędzi przeglądarki.

Skopiowane!

Informacje dodatkowe

Liczba arkuszy wydawniczych:140.00
Status:przed korektą
Rekord utworzony:6 lipca 2023 23:52
Ostatnia aktualizacja:6 lipca 2023 23:52